ϕ Paper detail :
Effect of temperature and exploitation time on tensile properties and plain strain fracture toughness, K Ic, in a welded
joint Ivica Čamagića , Simon Sedmakb *, Aleksandar Sedmakc , Zijah Burzićd , Mladen Marsenića a Faculty of Technical
Sciences, 7 Kneza Miloša Street, 38220 K. Mitrovica, Serbia b Innovation Center of the Faculty of Mechanical Engineering,
16 Kraljice Marije Street, 11120 Belgrade, Serbia c Faculty of Mechanical Engineering, 16 Kraljice Marije Street, 11120
Belgrade, Serbia d Military Technical Institute, 2 Ratka Resanovića Street, 11000 Belgrade, Serbia
ϕ Paper Source :
Available online at at www.sciencedirect.com
ϕ Succinct of the paper :
By reading this paper we have studied the testing results of tensile properties of specimens taken from the welded joint
of the new PM(parent metal) and WM (weld metal), from which now we can concluded that increased temperature
reduces strength properties, but increases elongation. The increase of elongation with the temperature increase is
explained by the increased overall plasticity of the material at higher temperatures. Also, the exploitation time significantly
impacts the reduction of strength properties and strain properties, which can be related to the microstructures of the
exploited and new PM. Based on the results in the paper we come up with conclusion that the lowest resistance to the
crack propagation, not surprisingly, belongs to HAZ (heat effected zone), whereas the highest resistance to crack
propagation, somewhat surprisingly, belongs to WM.
ϕ References :
ASTM E 1290-89, Standard Test Method for Crack-Tip Opening Displacement (CTOD) Fracture Toughness
Measurement, Annual Book of ASTM Standards, Vol. 03.01, 1993
ASTM E 1737-96, Standard Test Method for J Integral Characterization of Fracture Toughness, Annual Book of ASTM
Standards, Vol.03.01., 1996
ASTM E 1820-99a, Standard Test Method for Measurement of Fracture Toughness, Annual Book of ASTM Standards,
Vol. 03.01, 1999.
ASTM E1152-91, Standard Test Method for Determining J-R Curve, Annual Book of ASTM Standards, Vol. 03.01. p. 724,
1995.
ASTM E399-89, Standard Test Method for Plane-Strain Fracture Toughness of Metallic Materials, Annual Book of ASTM
Standards, Vol. 03.01. p. 522. 1986.
ASTM E813-89, Standard Test Method for JIc, A Measure of Fracture Toughness, Annual Book of ASTM Standards, Vol.
03.01. p. 651, 1993.
BS 5762-DD 19, Standard Test Method for Crack Opening Displacement, London, 1976.
BS 7448-Part 1, Fracture mechanics toughness tests-Method for determination of KIc critical CTOD and critical J values
of metallic materials, BSI, 1991.
BS 7448-Part 2, Fracture mechanics toughness tests - Methods for determination of KIc, critical CTOD and critical J
values of welds in metallic materials, BBI, 1997.
Burzić, Z., 2002. Savremene metode provere mehaničko-tehnoloških osobina zavarenih spojeva-Deo 2, Zavarivanje i
zavarene konstrukcije, 47(3), 151-158.
Čamagić, I., 2013. Investigation of the effects of exploitation conditions on the structural life and integrity assessment
of pressure vessels for high temperatures (in Serbian), doctoral thesis, Faculty of Technical Sciences, Kosovska
Mitrovica.
Camagic, I., Burzic, Z., Sedmak, A., Dascau, H., Milovic, L. 2015. Temperature effect on a low-alloyed steel welded joints
tensile properties, The 3rd IIW South – East European Welding Congress, “Welding & Joining Technologies for a
Sustainable Development & Environment”, Timisoara, Romania, Proceedings (77-81).
ESIS Procedure for Determining the Fracture Behavior of Materials, European Structural Integrity Society ESIS P2-92,
1992.
SRPS EN 10002-1, Metallic materials - Tensile testing - Part 1: Method of test (at ambient temperature), 1996.
SRPS EN 10002-5, Metallic materials - Tensile testing - Part 5: Method of testing at elevated temperature, 1997.
SRPS EN 895:2008, Destructive tests on welds in metallic materials - Transverse tensile test, 2008.
SRPS EN ISO 9692-1:2012, Welding and allied processes - Recommendations for joint preparation - Part 1: Manual
metal-arc welding, gas-shielded metal-arc welding, gas welding, TIG welding and beam welding of steels (ISO 9692-
1:2003), 2012.
SRPS EN ISO 9692-2:2008, Welding and allied processes - Joint preparation - Part 2: Submerged arc welding of steels
(ISO 9692-2:1998), 2008.