Abs GP-22

Terluran GP-22 is a commercial grade of Acrylonitrile Butadiene Styrene (ABS) from BASF, known for its high impact and heat deflection resistance, suitable for injection molding. It is available in North America and Europe, primarily used in telecommunications and automotive applications. The product features good flow properties and meets various ASTM and ISO test standards, with specific mechanical and thermal properties detailed in the document.

Uploaded by

marigelnitz
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
24 views2 pages

Abs GP-22

Terluran GP-22 is a commercial grade of Acrylonitrile Butadiene Styrene (ABS) from BASF, known for its high impact and heat deflection resistance, suitable for injection molding. It is available in North America and Europe, primarily used in telecommunications and automotive applications. The product features good flow properties and meets various ASTM and ISO test standards, with specific mechanical and thermal properties detailed in the document.

Uploaded by

marigelnitz
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 2

Terluran® GP-22 data provided by IDES Page 1 of 2

Terluran® GP-22
BASF Corporation - Acrylonitrile Butadiene Styrene

Product Description
Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat
deflection.
Product Characteristics
Material Status l Commercial: Active
Availability l North America
l Europe
Test Standards l ASTM
Available l ISO 10350
Recycled Content l No
Features l Copolymer l General Purpose
l Flow, Good l Impact Resistance, High

Uses l Telecommunications l Automotive Applications


l Housings l General Purpose
Automotive l FORD ESF-M4D241-B
Specifications l GM GMP.ABS.001
l FORD WSK -M4D827 -A
l FORD ESF-M4D236-A
l CHRYSLER MSDB 200 CPN4030
Forms l Pellets

Processing Method l Injection Molding

Multi-Point Data l Creep Modulus vs. Time (ISO 11403-1)


l Shear Modulus vs. Temperature (ISO
l Isochronous Stress vs. Strain (ISO
11403-2)
11403-1) l Specific Volume vs Temperature (ISO
l Isothermal Stress vs. Strain (ISO
11403-2)
11403-1) l Viscosity vs. Shear Rate (ISO 11403-2)
l Secant Modulus vs. Strain (ISO 11403-
1)
1
Properties
Physical Nominal Values (English) Test Method
Density 1.04 g/cm³ ASTM D1505
Mechanical Nominal Values (English) Test Method
Tensile Modulus 2 341000 psi ASTM D638
Tensile Strength @ Yield 3 6530 psi ASTM D638
Tensile Strength @ Break 3 4930 psi ASTM D638
Tensile Elongation @ Yld 2.6 % ASTM D638
Flexural Modulus 334000 psi ASTM D790
Flexural Strength 4 9430 psi ASTM D790
Impact Nominal Values (English) Test Method
Notched Izod Impact ASTM D256
(-40 °F, 0.125 in) 1.12 ft-lb/in
(0 °F, 0.125 in) 1.87 ft-lb/in
(73 °F, 0.125 in) 5.62 ft-lb/in
Hardness Nominal Values (English) Test Method
Rockwell Hardness (R-Scale) 103 ASTM D785
Thermal Nominal Values (English) Test Method
DTUL @264psi - Annealed (0.250 in) 210 °F ASTM D648
DTUL @264psi - Unannealed (0.250 in) 172 °F ASTM D648
DTUL @66psi - Annealed (0.250 in) 219 °F ASTM D648
DTUL @66psi - Unannealed (0.250 in) 196 °F ASTM D648
Vicat Softening Point (Rate A) 207 °F ASTM D1525
Terluran® GP-22 data provided by IDES Page 2 of 2

Ignition Characteristics Nominal Values (English) Test Method


Flame Rating - UL UL 94
(0.0590 in, ALL) HB
(0.118 in, ALL) HB
(0.0310 in, ALL) HB
UL 746 Nominal Values (English) Test Method
Rel Temp Indx Mech w/oImp UL 746
(0.0590 in) 203 °F
(0.118 in) 203 °F
(0.0310 in) 203 °F
Rel Temp Indx Mech w/Imp UL 746
(0.0310 in) 176 °F
(0.0590 in) 176 °F
(0.118 in) 176 °F
Rel Temp Indx Elect UL 746
(0.0310 in) 194 °F
(0.0590 in) 194 °F
(0.118 in) 194 °F
Additional Properties
Melt Flow Index, ASTM D1238, 220°C/10 kg: 19.6 g/10 min
Melt Flow Index, ASTM D1238, 230°C/3.8 kg: 4.7 g/10 min

Processing Information
Injection Molding Parameters Nominal Values (English) Test Method
Drying Temperature 176 °F
Drying Time 2.0 to 4.0 hr
Suggested Max Regrind 20 %
Processing (Melt) Temp 428 to 500 °F
Mold Temperature 86.0 to 140 °F

Notes
1 Typical properties; not to be construed as specifications.
2 0.125 in
3 Type I, 0.125 in
4 0.125 in