Typical Data:
Product Data
Properties
NE-5140 NE-5150 NE-5160 NE-5170 NE-5180 Test Method
Milk-white, light yellow, light gray, Visual
Appearance
no obvious extraneous matter. Inspection
1.10~ 1.13~ 1.16~ 1.19~ 1.20~
Density, g/cm3 ASTM D792
1.14 1.17 1.20 1.23 1.24
Hardness, Shore A 40±2 50±2 60±2 70±2 80±2 ASTM D2240
Tensile Strength, MPa ≥ 6.5 7.0 6.5 6.0
ASTM D412
Elongation at Break, % ≥ 420 320 280 200 150
Tension Set, % ≤ 8 6
Tear Strength, Die C kN/m ≥ 16 18 16 ASTM D624
Compression Set, 180℃*22h ≤ 40 35 30 ASTM D395
Resilience, % ≥ 60 50 45 /
● Physical data in the above table is for reference only.
● Vulcanization condition: 175℃*5Min.
● Ratio of curing agent liquid 2,5-Dimethyl-2,5-di(tert-butylperoxy)hexane: 0.65%.
●The supplied test report is obtained by the Quality Inspection Department with the curing conditions and testing
method of the company; due to the difference of curing conditions and testing method, we can’t guarantee that both
parties obtain the same testing result, and we suggest that users should use the test data obtained under their own testing
conditions as the reference for service performance. All the above performance data and application recommendations
are only a reference for use on the service performance of product, instead of a guarantee on the effectiveness or general
applicability of our products under a certain application.
Page No.2/2
Last Revision Date:2023.1
Version No.:2.0
Product Description: ECONOMIC SILICONE RUBBER FOR EXTRUSION
Characteristics:
● Good processability
Main Applications:
● Low-end miscellaneous extruded silicone rubber products.
Typical Data:
Product Data
Properties Test Method
NE-5240 NE-5250 NE-5260 NE-5270 NE-5280
Milk-white, light yellow, light gray, Visual
Appearance
no obvious extraneous matter. Inspection
1.10~ 1.13~ 1.16~ 1.19~ 1.20~
Density, g/cm3 ASTM D792
1.14 1.17 1.20 1.23 1.24
Hardness, Shore A 40±2 50±2 60±2 70±2 80±2 ASTM D2240
Tensile Strength, MPa ≥ 6.5 7.0 6.5 6.0
Elongation at Break, % ≥ 420 320 280 200 150 ASTM D412
Tension Set, % ≤ 10 8
Tear Strength, Die C kN/m ≥ 16 18 16 ASTM D624
Compression Set, 180℃*22h ≤ 40 35 30 ASTM D395
Resilience, % ≥ 50 45 /
● Physical data in the above table is for reference only.
● Vulcanization condition: 175℃* 5Min.
● Ratio of curing agent liquid 2,5-Dimethyl-2,5-di (tert- butylperoxy) hexane: 0.65%.
●The supplied test report is obtained by the Quality Inspection Department with the curing conditions and testing
method of the company; due to the difference of curing conditions and testing method, we can’t guarantee that both
parties obtain the same testing result, and we suggest that users should use the test data obtained under their own testing
conditions as the reference for service performance. All the above performance data and application recommendations